The furnace is designed to the user’s requirements for a proprietary sinter/heat treatment process and is equipped with three heating chambers to manage three different processes that include delubrication, sintering, and post-sintering heat treatment.

The delubrication system uses Sinterite’s Accelerated Delubrication System (ADS). The sintering zones use silicon carbide muffle sections in a gas tight heating chamber, and the cooling system is equipped with the Sinterite HyperCooler rapid cooling system.

The furnace operates at a maximum temperature of 2200°F (1200°C) and is capable of net production output of 1700 lbs (770 kg) per hour.