ALD Vacuum Technologies, based in Hanau, Germany, has supplied three high-pressure sintering furnaces to Xiamen Golden Egret Special Alloy Co Ltd.

Brazilian mining company Vale has rejected a four-year labour agreement proposed by the Labrador and Newfoundland provincial government to settle an 18-mon

China’s commerce Ministry has confirmed that the export quota for rare earth elements is to be cut by 35% in the first six months of 2011. Total exports wi

Researchers have developed a new metal nanomaterial for use in Li-ion batteries.

Blade manufacturer Fisher-Barton Group, based in Waukesha, Wisconsin, USA, has acquired Lineage Alloys, a thermal spray powder manufacturer located near Ho

Royal Metal Powders, Inc, a subsidiary of American Chemet Corp based in Maryville, Tennessee, USA, has installed a new air-atomization production unit.