Metal processing news, January 2014

Molycorp says that its Sillam?e, Estonia, tantalum smelter facility has been certified by the Electronic Industry Citizenship Coalition (EICC) and the Glob

First iron powder exports from China

Wuhan Iron and Steel Corporation (WISCO) has made its first international export of reduced iron powder.

The programme of events, speakers and workshops at the 2014 AMUG Conference is now available online.

Private equity firm Cyprium Partners has sold Alpha Sintered Metals Inc (ASM) to its management and to O2 Investment Partners, LLC, another private equity

Cristal Global and The National Industrialization Company (Tasnee) have signed an agreement to establish a joint venture (JV) company with Japanese titaniu

ASTM International has released a new edition of its Manual 32, Test Sieving Methods: Guidelines for Establishing Sieve Analysis Procedures, 5th Edition.

TAT Technologies has provided information about its famous four-day long hands-on sintering course, which takes place in 2014 from 25-28 February.

Miba AG has agreed to increase its interest in Mahle Metal Leve Miba Sinterizados Ltda in Indaiatuba, Brazil, by 10% from 30 to 40%.

The Industrial Heating Equipment Association (IHEA)'s infrared equipment division (IRED) is running a free educational webinar focused on infrared (IR) cur

The final unit of Molycorp’s cracking plant at its Mountain Pass molybdenum source has now completed commissioning and is operational.

Blackheath Resources Inc, a mining exploration and development company, has agreed an option to acquire a 100% interest in the Adoria tungsten/tin project

ASTM’s standard ASTM B330, used to measure the particle size of metal powders, now covers recent changes in PM testing technology.