Gasbarre Thermal Processing Systems has received three separate orders for batch steam treating equipment.
Gasbarre Thermal Processing Systems has received three separate orders for batch steam treating equipment.

Gasbarre Thermal Processing Systems has reportedly received three separate orders for batch steam treating equipment.

According to the company, the batch steam treaters produce an oxide layer that helps improve corrosion and wear resistance and provides a more attractive surface finish. The three orders range in size from 18’ to 30’ in diameter and 12’ to 48’ deep, with a gross load weight capacity ranges from 300 lbs to 1800 lbs. The equipment is electrically heated and has a maximum operating temperature rating of 1400°F.

Gasbarre says that the equipment will be shipped to companies in the medical, additive manufacturing, automotive and consumer products industries.