A team of scientists has made the strongest silver ever – 42% stronger than the previous world record holder. But that's not the important point.

"We've discovered a new mechanism at work at the nanoscale that allows us to make metals that are much stronger than anything ever made before – while not losing any electrical conductivity," says Frederic Sansoz, a materials scientist and mechanical engineering professor at the University of Vermont (UVM) who co-led the new discovery.

This fundamental breakthrough promises a new category of materials that can overcome a traditional trade-off in industrial and commercial materials between strength and the ability to carry electrical current. The team, which included experts from UVM, Lawrence Livermore National Laboratory, the Ames Laboratory, the Los Alamos National Laboratory and the University of California, Los Angeles, reports its findings in a paper in Nature Materials.

All metals have defects. Often these defects lead to undesirable qualities, like brittleness or softening. This has led scientists to create various alloys or heavy mixtures of metallic materials to make them stronger. But as they get stronger, they lose electrical conductivity.

"We asked ourselves, how can we make a material with defects but overcome the softening while retaining the electroconductivity," said Morris Wang, a lead scientist at Lawrence Livermore National Laboratory and co-author of the paper.

By mixing a trace amount of copper into the silver, the team showed that it can transform two types of inherent nanoscale defects into a powerful internal structure. "That's because impurities are directly attracted to these defects," explains Sansoz.

In other words, the team used a copper impurity – a form of doping or ‘microalloy’ as the scientists style it – to control the behavior of defects in silver. Like a kind of atomic-scale jiu-jitsu, the scientists flipped the defects to their advantage, using them to both strengthen the metal and maintain its electrical conductivity.

To make its discovery, the team started with a foundational idea of materials engineering: as the size of a crystal – or grain – of a material gets smaller, it gets stronger. Scientists call this the Hall-Petch relation. This general design principle has allowed scientists and engineers to build stronger alloys and advanced ceramics for over 70 years. It works very well.

Until it doesn't. Eventually, when grains of metal reach an infinitesimally tiny size – under tens of nanometers wide – the boundaries between the grains become unstable and begin to move. Therefore, another known approach to strengthening metals like silver uses nanoscale ‘coherent twin boundaries’, which are a special type of grain boundary. These structures of paired atoms – forming a symmetrical mirror-like crystalline interface – are exceedingly strong, allowing them to withstand deformation. Except that these twin boundaries, too, become soft when their interspacing falls under a critical size of a few nanometers, due to imperfections.

Very roughly speaking, nanocrystals are like patches of cloth and nanotwins are like strong but tiny threads in that cloth. Except they're at the atomic scale. The new research combines both approaches to make what the scientists call a ‘nanocrystalline-nanotwinned metal’ that has "unprecedented mechanical and physical properties," the team writes.

That's because the copper atoms, slightly smaller than the atoms of silver, move into defects in both the grain boundaries and the twin boundaries. This allowed the team – using computer simulations of atoms as a starting point and then moving into real metals with advanced instruments at the National Laboratories – to create the new super-strong form of silver. The tiny copper impurities within the silver inhibit the defects from moving, but are such a small amount of metal – less than 1% of the total – that the rich electrical conductivity of silver is retained.

"The copper atom impurities go along each interface and not in between," Sansoz explains. "So they don't disrupt the electrons that are propagating through."

Not only does this copper-laced silver overcome the softening previously observed as grains and twin boundaries get too small – the so-called ‘Hall-Petch breakdown’ – it even exceeds the long-standing theoretical Hall-Petch limit. The team reports that an ‘ideal maximum strength’ can be found in metals with twin boundaries that are under 7nm apart, just a few atoms. And a heat-treated version of the copper-laced silver has a hardness measure above what had been thought to be the theoretical maximum.

"We've broken the world record, and the Hall-Petch limit too, not just once but several times in the course of this study, with very controlled experiments," says Sansoz.

Sansoz is confident that the team's approach to making super-strong and still-conductive silver can be applied to many other metals. "This is a new class of materials and we're just beginning to understand how they work," he says. And he anticipates that the basic science revealed in the new study can lead to advances in various technologies – from more efficient solar cells to lighter airplanes to safer nuclear power plants.

"When you can make material stronger, you can use less of it, and it lasts longer," he says, "and being electrically conductive is crucial to many applications."

This story is adapted from material from the University of Vermont, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.