Peng Wei is a condensed-matter physicist at UCR, studying quantum states of electrons in new materials. Photo: I. Pittalwala, UC Riverside.A joint team of scientists at the University of California, Riverside (UCR) and the Massachusetts Institute of Technology (MIT) is getting closer to confirming the existence of an exotic quantum particle called a Majorana fermion. This quantum particle could be crucial for fault-tolerant quantum computing – the kind of quantum computing that addresses errors during its operation.
Quantum computing uses quantum phenomena to perform computations. Majorana fermions exist at the boundary of special superconductors called topological superconductors, which have a superconducting gap in their interiors and harbor Majorana fermions outside, at their boundaries. Majorana fermions are one of the most sought-after objects in quantum physics because they are their own antiparticles, they can split the quantum state of an electron in half and they follow different statistics compared to electrons. Though many have claimed to have identified them, scientists still cannot confirm their exotic quantum nature.
The UCR-MIT team overcame this challenge by developing a new heterostructure material system, based on gold, that could potentially be used to demonstrate the existence and quantum nature of Majorana fermions. Heterostructure materials are made up of layers of drastically dissimilar materials that, when stacked together, show completely different functionalities to their individual layers.
"It is highly nontrivial to find a material system that is naturally a topological superconductor," said Peng Wei, an assistant professor of physics and astronomy and a condensed matter experimentalist at UCR, who co-led the study with Jagadeesh Moodera and Patrick Lee at MIT. "A material needs to satisfy several stringent conditions to become a topological superconductor." Wei and his team report their findings in a paper in Physical Review Letters.
The Majorana fermion, considered to be half of an electron, is predicted to be found at the ends of a topological superconductor nanowire. Interestingly, two Majorana fermions can combine with each other to make up one electron, allowing the quantum states of the electron to be stored nonlocally – an advantage for fault-tolerant quantum computing.
In 2012, MIT theorists, led by Lee, predicted that heterostructures of gold can become a topological superconductor under strict conditions. Experiments done by the UCR-MIT team have now achieved all the necessary conditions for such heterostructures of gold.
"Achieving such heterostructure is highly demanding because several material physics challenges needed to be addressed first," said Wei, a UCR alumnus who returned to campus in 2016 from MIT.
According to Wei, the research paper shows that superconductivity, magnetism and electrons' spin-orbit coupling can co-exist in gold – a difficult challenge to meet – and be manually mixed with other materials through heterostructures. "Superconductivity and magnetism ordinarily do not coexist in the same material," he said.
Gold is not a superconductor, he added, and neither are the electron states on its surface. "Our paper shows for the first time that superconductivity can be brought to the surface states of gold, requiring new physics. We show that it is possible to make the surface state of gold a superconductor, which has never been shown before."
The research paper also shows that the electron density of superconductivity in the surface states of gold can be tuned. "This is important for future manipulation of Majorana fermions, required for better quantum computing," Wei said. "Also, the surface state of gold is a two-dimensional system that is naturally scalable, meaning it allows the building of Majorana fermion circuits."
This story is adapted from material from the University of California, Riverside, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.