Engineers at Rice University have designed a catalyst of ruthenium atoms in a copper mesh to extract ammonia and fertilizer from wastewater. Photo: Jeff Fitlow/Rice University.A dash of ruthenium atoms on a mesh of copper nanowires could represent a step towards a revolution in the global ammonia industry that also helps the environment. Developed by researchers from Rice University’s George R. Brown School of Engineering, Arizona State University and Pacific Northwest National Laboratory, this high-performance catalyst can, with near 100% efficiency, extract ammonia and solid ammonia – aka fertilizer – from low levels of nitrates that are widespread in industrial wastewater and polluted groundwater.
A study led by Rice chemical and biomolecular engineer Haotian Wang shows that this catalytic process can convert nitrate levels of 2000 parts per million into ammonia, followed by an efficient gas stripping process for ammonia product collection. The nitrogen that remains in the water after these treatments can be brought down to ‘drinkable’ levels as defined by the World Health Organization.
“We fulfilled a complete water denitrification process,” said graduate student Feng-Yang Chen. “With further water treatment on other contaminants, we can potentially turn industrial wastewater back to drinking water.” Chen is one of three lead authors of a paper on this work in Nature Nanotechnology.
The study demonstrates a promising alternative approach towards efficient processes for an industry that currently depends upon an energy-intensive process to produce more than 170 million tons of ammonia per year.
The researchers knew from previous studies that ruthenium atoms are champs at catalyzing nitrate-rich wastewater. Their twist was combining it with copper to suppress the hydrogen evolution reaction, a way to produce hydrogen from water that in this case is an unwanted side effect.
“We knew that ruthenium was a good metal candidate for nitrate reduction, but we also knew there was a big problem, that it could easily have a competing reaction, which is hydrogen evolution,” Chen said. “When we applied current, a lot of the electrons would just go to hydrogen, not the product we want.”
“We borrowed a concept from other fields like carbon dioxide reduction, which uses copper to suppress hydrogen evolution,” explained Wang. “Then we had to find a way to organically combine ruthenium and copper. It turns out that dispersing single ruthenium atoms into the copper matrix works the best.”
According to co-corresponding author Christopher Muhich, an assistant professor of chemical engineering at Arizona State University, the team used density functional theory calculations to explain why ruthenium atoms make the chemical path connecting nitrate and ammonia easier to cross.
“When there is only ruthenium, the water gets in the way,” Muhich said. “When there is only copper, there isn’t enough water to provide hydrogen atoms. But on the single ruthenium sites water doesn’t compete as well, providing just enough hydrogen without taking up spots for nitrate to react.”
The catalytic process works at room temperature and under ambient pressure, and at what the researchers called an ‘industrial-relevant’ nitrate reduction current of 1 amp per square centimeter, the amount of electricity needed to maximize the catalysis rate. That should make it easy to scale up, Chen said.
“I think this has big potential, but it’s been ignored because it’s been hard for previous studies to reach such a good current density while still maintaining good product selectivity, especially under low nitrate concentrations,” he added. “But now we’re demonstrating just that. I’m confident we’ll have opportunities to push this process for industrial applications, especially because it doesn’t require big infrastructure.”
A prime benefit of the process is the potential for reducing carbon dioxide emissions from the traditional industrial production of ammonia. These are not insignificant, amounting to 1.4% of the world’s annual emissions, the researchers noted.
“While we understood that converting nitrate wastes to ammonia may not be able to fully replace the existing ammonia industry in the short term, we believe this process could make significant contributions to decentralized ammonia production, especially in places with high nitrate sources,” Wang said.
This story is adapted from material from Rice University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.