The unassuming piece of stainless steel mesh in a lab at The Ohio State University doesn’t look like a very big deal, but it could make a big difference for future environmental cleanups.
Water passes through the mesh but oil doesn’t, thanks to a nearly invisible oil-repelling coating on its surface.
In tests, researchers mixed water with oil and poured the mixture onto the mesh. The water filtered through the mesh to land in a beaker below. The oil collected on top of the mesh, and rolled off easily into a separate beaker when the mesh was tilted.
The mesh coating is among a suite of nature-inspired nanotechnologies under development at Ohio State and described in two papers (here and here) in the journal Nature Scientific Reports. Potential applications range from cleaning oil spills to tracking oil deposits underground.
“If you scale this up, you could potentially catch an oil spill with a net,” said Bharat Bhushan, Ohio Eminent Scholar and Howard D. Winbigler Professor of mechanical engineering at Ohio State.
The work was partly inspired by lotus leaves, whose bumpy surfaces naturally repel water but not oil. To create a coating that did the opposite, Bhushan and postdoctoral researcher Philip Brown chose to cover a bumpy surface with a polymer embedded with molecules of surfactant—the stuff that gives cleaning power to soap and detergent.
They sprayed a fine dusting of silica nanoparticles onto the stainless steel mesh to create a randomly bumpy surface and layered the polymer and surfactant on top.
The silica, surfactant, polymer, and stainless steel are all non-toxic and relatively inexpensive, said Brown. He estimated that a larger mesh net could be created for less than a dollar per square foot.
Because the coating is only a few hundred nanometers (billionths of a meter) thick, it is mostly undetectable. To the touch, the coated mesh doesn’t feel any bumpier than uncoated mesh. The coated mesh is a little less shiny, though, because the coating is only 70 percent transparent.
The researchers chose silica in part because it is an ingredient in glass, and they wanted to explore this technology’s potential for creating smudge-free glass coatings. At 70 percent transparency, the coating could work for certain automotive glass applications, such as mirrors, but not most windows or smartphone surfaces.
“Our goal is to reach a transparency in the 90-percent range,” Bhushan said. “In all our coatings, different combinations of ingredients in the layers yield different properties. The trick is to select the right layers.”
He explained that certain combinations of layers yield nanoparticles that bind to oil instead of repelling it. Such particles could be used to detect oil underground or aid removal in the case of oil spills.
This story is reprinted from material from The Ohio State University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.