Most people value large chunks of gold – but scientists at the Vienna University of Technology are interested in gold at the smallest possible scale, because single gold atoms are potentially the most reactive catalysts for chemical reactions. However, when gold atoms are placed on a surface they tend to ball up into tiny nuggets consisting of several atoms. A team of surface scientists now managed to fix single gold atoms on special sites of an iron-oxide surface. This could open the door to more efficient catalysts, requiring less of the precious material.
Gold is a noble metal and does not usually bond with other elements, but as a catalyst it facilitates chemical reactions. It can, for example, facilitate the conversion of poisonous carbon monoxide to carbon dioxide. The effectiveness of gold as a catalyst depends on the size of the gold particles. Some evidence suggests that it works best if the gold is present in the form of single atoms. So far, however, this could not be studied in detail. “If individual gold atoms are put on a surface, they usually cluster up, forming nanoparticles”, says Gareth Parkinson, who oversaw the experiments in the research group of Professor Ulrike Diebold at the Institute for Applied Physics at the TU Vienna.
Higher temperatures lead to a higher mobility of the gold atoms, so in order to stop the atoms from clustering, most surfaces must be cooled to a temperature so low that the desired chemical reactions would stop entirely. The researchers at the TU Vienna found a special kind of iron-oxide surface, which locks the single gold atoms in place.
The key to success is a slight deformation of the iron-oxide crystal structure. The oxygen atoms of the topmost layer are not aligned in perfectly straight lines, they are bent into wiggles by the atoms below. At the points where the lines of oxygen atoms are close to each other, the gold atoms attach permanently without losing grip. Even if the surface is heated, the gold atoms stay put – only at 500 degrees celsius they start forming clusters.
“When a gold atom hits the iron oxide surface, it diffuses to one of the sites where it can be attached to the surface”, says Gareth Parkinson. That way, many single gold atoms can be placed close to each other. When a gold atom hits a position already occupied by another gold atom, however, the two bond and start moving across the surface, picking up additional gold atoms along the way. When they have reached a critical size of at least five atoms, they become immobile again and the miniature gold nugget comes to rest.
Ulrike Diebold expects that the new method will answer important open questions about catalysis. “We have created an ideal model system for probing the chemical reactivity of single atomic species”, says Diebold. The recent experiments will also help to advance theoretical research: the quantum mechanically complex bonding between single atoms and this particular surfaces provide an excellent test case for theoretical calculations of highly correlated electron systems.
This story is reprinted from material from Vienna University of Technology, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.