The Titanium Industry Development Association (TiDA) has opened a new facility in New Zealand designed to develop new titanium products.
29 June 2010

Janicki Industries, based in Sedro-Woolley, Washington, USA has built a giant 1600°F/871°C annealing furnace, designed to handle large-scale, high-precisio