Bodycote Plc is expanding its hot isostatic pressing capacity with investments in the USA.

MV Products has introduced a multiple stage vacuum inlet trap that protects vacuum pumps in metal injection moulding (MIM), vacuum compression moulding, an

Böhler Edelstahl is expanding its metal powder capacity in a two-year investment project totalling €16 million.

PowderMet 2012, to be held in Nashville, Tennessee, USA, on 10-13 June, is now open for registrations.

Thermal Technology has built a graphite 500,000 pound force capacity hot press to produce large powder metallurgy semiconductor materials.

Polymer Technologies Inc. (PTI), which specialises in plastic and metal injection moulding, is acquiring the Wallington, NJ-based manufacturer and repair s

The deadline for registering at a discount for the MIM2012 International Conference on Injection Moulding of Metals, Ceramics and Carbide, is 17 February.

Sumitomo Electric Industries Ltd is launching micromachining cutting tools tipped with nano-polycrystalline diamond, Sumidia Binderless.

Uralelectromed, a subsidiary of Russia's Ural Mining & Metallurgical Company, is expanding its powder metal capacity by installing new presses and a sinter