Additive manufacturing (AM) company Arcam AB, says that its powder manufacturing subsidiary AP&C, based in Montreal, Canada, has received a significant order for MIM (metal injection molding) applications.

This order, which is for Ti6Al4V MIM powder, establishes AP&C as a major supplier in the MIM application field. The order volume of 30 tons is to be delivered during 2017.

This story uses material from Arcam, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.