With a measuring range of X = 700 mm, Y = 1000 mm, and Z = 600 mm, this new equipment is able to measure a wide variety of metal components with a degree of accuracy of .00008 in over 3 in. It can measure precision machined components, tooling, and wire EDM components to tight tolerances with high accuracy and repeatability.



Garner Industries

selected the Zeiss CONTURA G2 because it is a very robust machine design with the benefits of high-speed scanning. It features a flexible articulating probe that offers scanning in all angular positions to provide a highly accurate and concentrated acquisition of measuring points that is much more reliable, robust and reproducible than conventional systems, the company says.