An official call for presentations has been announced for MIM2019, International Conference on Injection Molding of Metals, Ceramics and Carbides, held in Orlando, Florida from 25–27 February 2019.

Authors have until 28 September 2018, to submit presentation abstracts on manufacturing innovations and material advancements.

Sponsored by the Metal Injection Molding Association, a trade association of the Metal Powder Industries Federation (MPIF) and its affiliate APMI International, MIM2019 is suitable for product designers, engineers, end users, manufacturers, researchers, educators, and students.