“Ultrahigh-Strength Sinter-Hardening MIM Alloy Steels”, authored by Kuen-Shyang Hwang, Chen Hsu, and Li-Hui Cheng from Taiwan National University, and Po-Han Chen of Taiwan Powder Technologies Co, was one of 19 qualified manuscripts that were presented at the PowderMet2011 conference which were evaluated for the award.
 
The authors will receive award plaques during the PowderMet2012 conference in Nashville, Tennessee, USA, which will take place from 10–13 June 2012. The paper will be published in the conference proceedings, Advances in Powder Metallurgy & Particulate Materials2011.