Parmatech manufactures MIM components used in a variety of bariatric and laparoscopic instruments and orthodontics that take advantage of MIM’s miniaturisation and intricate shape capability.

Applications also include sealing and transecting of blood vessels and vein harvesting for bypass surgeries.

Parmatech Corporation is part of the ATW family of companies.