Dr Randal M German, Professor of Mechanical Engineering at San Diego University and a specialist in powder injection molding (PIM), will give a one tutorial during PM China, taking place from 27–29 April 2016 in Shanghai.

Dr German will choose topics that most concerned the PM & MIM communities in China and plans to supply tutorial material both in English and Chinese for better understanding and communication in the audience.

His teaching and research interests are in the area of powder metallurgy, sintering, materials processing, ceramics, in particular, engineering materials and their net-shape fabrication based on techniques such as powder metallurgy, injection molding, and advanced ceramic forming  technologies.?