The kit can measure the laser power before and after a building job, and during production the laser power is tracked. The results are reported in the EOSTATE 1.2 Quality Assurance module.

EOS has already developed the EOSINT M 280 Comfort Powder Module, a new module of the IPCM-M, which enables more comfortable powder handling with a closed process chamber, thus lowering the risk of exposure to the powder.