Self crimped and aligned fibers
Volume 14, Issue 5, Page 226–229
| Thinakaran Senthilram, Loordhuswamy Amalorpava Mary, Jayarama Reddy Venugopal, Lakshmanan Nagarajan, Seeram Ramakrishna, Venkateshwarapuram Rengaswami Giri Dev
Electrospinning is one of the most successful means of producing nanofibers with enormous application potential. New methods of producing nanofibers without high voltages are presently being explored by researchers around the globe. In the present work, a facile method of producing aligned and crimped fibers with polycaprolactone by rotating the needle assembly is described.