Illustration of a novel room-temperature process for removing carbon dioxide by converting it into carbon monoxide. Instead of using heat, the nanoscale method relies on the energy from surface plasmons (violet hue) that are excited when a beam of electrons (vertical beam) strikes aluminum nanoparticles resting on graphite. Aided by the energy derived from the plasmons, carbon dioxide molecules (black dot bonded to two red dots) are converted to carbon monoxide (black dot bonded to one red dot). The hole under the violet sphere represents the graphite etched away during the chemical reaction. Image: NIST.A team led by researchers at the US National Institute of Standards and Technology (NIST) has demonstrated a room-temperature method for significantly reducing carbon dioxide levels in fossil-fuel power plant exhaust, one of the main sources of carbon emissions to the atmosphere.
Although the researchers demonstrated this method in a small-scale, highly controlled environment with dimensions of just nanometers, they have already come up with ideas for scaling up the method and making it practical for real-world applications.
In addition to offering a potential new way of mitigating the effects of climate change, the chemical process employed by the scientists could also reduce the costs and energy requirements for producing liquid hydrocarbons and other chemicals used by industry. That's because the method's by-products include the building blocks for synthesizing methane, ethanol and other carbon-based compounds used in industrial processing.
The team's method taps a novel energy source from the nanoworld to trigger a run-of-the-mill chemical reaction that eliminates carbon dioxide. In this reaction, solid carbon latches onto one of the oxygen atoms in carbon dioxide gas, reducing it to carbon monoxide. The reaction normally requires significant amounts of energy in the form of high heat – a temperature of at least 700°C, hot enough to melt aluminum at normal atmospheric pressure.
Instead of heat, the team relied on the energy harvested from traveling waves of electrons, known as localized surface plasmons (LSPs), which surf on individual aluminum nanoparticles. The team triggered the LSP oscillations by exciting the nanoparticles with an electron beam that had an adjustable diameter. A narrow beam, about a nanometer in diameter, bombarded individual aluminum nanoparticles, while a beam about a thousand times wider generated LSPs among a large set of the nanoparticles.
In the team's experiment, the aluminum nanoparticles were deposited on a layer of graphite, a form of carbon. This allowed the nanoparticles to transfer their LSP energy to the graphite. In the presence of carbon dioxide gas, which the team injected into the system, the graphite was able to pluck individual oxygen atoms from the carbon dioxide, reducing it to carbon monoxide. All the while, the aluminum nanoparticles were kept at room temperature. In this way, the team accomplished a major feat: getting rid of the carbon dioxide without the need for a source of high heat.
Previous methods for removing carbon dioxide have had limited success because the techniques have required high temperatures or pressures, employed costly precious metals, or had poor efficiency. In contrast, the LSP method not only saves energy but also uses aluminum, a cheap and abundant metal.
Although the LSP reaction generates a poisonous gas – carbon monoxide – this gas readily combines with hydrogen to produce essential hydrocarbon compounds, such as methane and ethanol, that are often used in industry, said NIST researcher Renu Sharma. She and her colleagues, including scientists from the University of Maryland and DENSsolutions in Delft, the Netherlands, report their findings in a paper in Nature Materials.
"We showed for the first time that this carbon dioxide reaction, which otherwise will only happen at 700°C or higher, can be triggered using LSPs at room temperature," said researcher Canhui Wang of NIST and the University of Maryland.
The researchers chose an electron beam to excite the LSPs because the beam can also be used to image structures in the system as small as a few billionths of a meter via transmission electron microscopy (TEM). This allowed the team to estimate how much carbon dioxide had been removed.
Because both the concentration of carbon dioxide and the reaction volume of the experiment were so small, the researchers had to take special steps to directly measure the amount of carbon monoxide generated. They did so by coupling a specially modified gas cell holder from the TEM to a gas chromatograph-mass spectrometer, allowing them to measure parts-per-million concentrations of carbon monoxide.
Sharma and her colleagues also used the images produced by the electron beam to measure the amount of graphite that was etched away during the experiment, a proxy for how much carbon dioxide had been removed. They found that the ratio of carbon monoxide to carbon dioxide measured at the outlet of the gas cell holder increased linearly with the amount of carbon removed by etching.
Imaging with the electron beam also confirmed that most of the carbon etching occurred near the aluminum nanoparticles. Additional studies revealed that when the aluminum nanoparticles were absent from the experiment, only about one-seventh as much carbon was etched.
Limited by the size of the electron beam, the team's experimental system was small, only about 15–20nm across (the size of a small virus). To scale up the system so that it could remove carbon dioxide from the exhaust of a commercial power plant, a light beam may be a better choice than an electron beam to excite the LSPs, Wang said.
Sharma proposes that a transparent enclosure containing loosely packed carbon and aluminum nanoparticles could be placed over the smokestack of a power plant. An array of light beams impinging upon the grid would activate the LSPs. When the exhaust passes through the device, the light-activated LSPs in the nanoparticles would provide the energy to remove carbon dioxide.
The aluminum nanoparticles, which are commercially available, should be evenly distributed to maximize contact with the carbon source and the incoming carbon dioxide, the team noted.
This new work also suggests that LSPs could offer a way for a slew of other chemical reactions that now require a large infusion of energy to proceed at ordinary temperatures and pressures using plasmonic nanoparticles. "Carbon dioxide reduction is a big deal, but it would be an even bigger deal, saving enormous amounts of energy, if we can start to do many chemical reactions at room temperature that now require heating," Sharma said.
This story is adapted from material from NIST, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.