Scientists at the University of Birmingham, really took Valentine's day to heart this year and made possibly the smallest Valentines day card ever. Made of pure palladium it is only 8 nanometers in size. You might say making the card was also a work of love; clusters of palladium atoms bonded together on the surface of carbon and spontaneously arranged into the worlds smallest heart.