In lab tests, skin patches covered by graphene films got zero mosquito bites, while mosquitoes readily feasted on unprotected skin. Image: Hurt Lab/Brown University.
In lab tests, skin patches covered by graphene films got zero mosquito bites, while mosquitoes readily feasted on unprotected skin. Image: Hurt Lab/Brown University.

The nanomaterial graphene has received significant attention for its potential uses in everything from solar cells to tennis rackets. But a new study by researchers at Brown University has found a surprising new use for the material: preventing mosquito bites.

In a paper in the Proceedings of the National Academy of Sciences, the researchers report that multilayer graphene can provide a two-fold defense against mosquito bites. The ultra-thin yet strong material acts as a barrier that mosquitoes are unable to bite through. At the same time, experiments showed that graphene also blocks the chemical signals mosquitoes use to sense that a blood meal is near, blunting their urge to bite in the first place. The findings suggest that clothing with a graphene lining could be an effective mosquito barrier.

"Mosquitoes are important vectors for disease all over the world, and there's a lot of interest in non-chemical mosquito bite protection," said Robert Hurt, a professor in Brown's School of Engineering and senior author of the paper. "We had been working on fabrics that incorporate graphene as a barrier against toxic chemicals, and we started thinking about what else the approach might be good for. We thought maybe graphene could provide mosquito bite protection as well."

To find out if it would work, the researchers recruited some brave participants willing to get a few mosquito bites in the name of science. The participants placed their arms in a mosquito-filled enclosure so that only a small patch of their skin was available to the mosquitoes for biting. The mosquitoes were bred in the lab so they could be confirmed to be disease-free.

The researchers compared the number of bites participants received on their bare skin, on skin covered in cheesecloth and on skin covered by graphene oxide (GO) films sheathed in cheesecloth. GO is a graphene derivative that can be made into films large enough for macro-scale applications.

They quickly discovered that graphene was an effective bite deterrent. When skin was covered by dry GO films, participants didn't get a single bite, while bare and cheesecloth-covered skin was readily feasted upon. What was surprising, the researchers said, was that the mosquitoes completely changed their behavior in the presence of the graphene-covered arm.

"With the graphene, the mosquitoes weren't even landing on the skin patch – they just didn't seem to care," said Cintia Castilho, a PhD student at Brown and the study's lead author. "We had assumed that graphene would be a physical barrier to biting, through puncture resistance, but when we saw these experiments, we started to think that it was also a chemical barrier that prevents mosquitoes from sensing that someone is there."

To confirm the chemical barrier idea, the researchers dabbed some human sweat onto the outside of a graphene barrier. With the chemical cues on the outside of the graphene, the mosquitoes flocked to the patch in much the same way they flocked to bare skin.

Other experiments showed that GO can also provide puncture resistance – but not all the time. Using a tiny needle as a stand-in for a mosquito's proboscis, as well as computer simulations of the bite process, the researchers showed that mosquitoes simply can't generate enough force to puncture GO. But that only applied when the GO is dry.

The simulations found that GO would be vulnerable to puncture when it was saturated with water. And sure enough, experiments showed that mosquitoes could bite through wet GO. However, another form of GO with reduced oxygen content (called rGO) was shown to provide a bite barrier when both wet and dry.

A next step for the research will be to find a way to stabilize the GO so that it's tougher when wet, Hurt says. That's because GO has a distinct advantage over rGO when it comes to wearable technology.

"GO is breathable, meaning you can sweat through it, while rGO isn't," Hurt said. "So, our preferred embodiment of this technology would be to find a way to stabilize GO mechanically so that it remains strong when wet. This next step would give us the full benefits of breathability and bite protection."

All told, the researchers say, the study suggests that properly engineered graphene linings could be used to make mosquito-protective clothing.

This story is adapted from material from Brown University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.