This illustrates the new, scalable production system for creating MXene materials in batches as large as 50g. Image: Drexel University.For more than a decade, two-dimensional (2D) nanomaterials, such as graphene, have been touted as the key to making better microchips, batteries, antennas and many other devices. But a significant challenge of using these atom-thin building materials for the technology of the future is ensuring they can be produced in bulk quantities without losing their quality.
For one of the most promising new types of 2D nanomaterials, MXenes, that's no longer a problem. Researchers at Drexel University and the Materials Research Center in Ukraine have designed a system that can be used to make large quantities of this nanomaterial while preserving its unique properties.
In a paper in Advanced Engineering Materials, the team reports that a lab-scale reactor system developed at the Materials Research Center in Kyiv can convert a ceramic precursor material into a pile of the powdery black MXene titanium carbide, in quantities as large as 50g per batch.
Proving that large batches of material can be refined and produced with consistency is a critical step toward achieving viability for manufacturing. For MXene materials, which have already shown their potential in prototype devices for energy storage, computing, communication and health care, reaching manufacturing standards is the home stretch on the way to mainstream use.
"Proving a material has certain properties is one thing, but proving that it can overcome the practical challenges of manufacturing is an entirely different hurdle – this study reports on an important step in this direction," said Yury Gogotsi, professor in Drexel's College of Engineering, who has pioneered the research and development of MXene and is a lead author of the paper. "This means that MXene can be considered for widespread use in electronics and energy storage devices."
Researchers at Drexel have been making MXene in small quantities – typically 1g or less – since they first synthesized the material in 2011. This layered nanomaterial, which looks like a powder in its dry form, starts as a piece of ceramic called a MAX phase. When a mixture of hydrofluoric and hydrochloric acid interacts with this MAX phase, it etches away certain parts of the material, creating the nanometer-thin flakes characteristic of MXenes.
In the lab, this process takes place in a 60ml container with the ingredients added and mixed by hand. To more carefully control the process at a larger scale, the group uses a 1L reactor chamber and a screw feeder device to precisely add MAX phase. One inlet feeds the reactants uniformly into the reactor and another allows for gas pressure relief during the reaction. A specially designed mixing blade ensures thorough and uniform mixing. And a cooling jacket around the reactor lets the team adjust the temperature of the reaction. The entire process is computerized and controlled by a software program created by the Materials Research Center team.
The group reports using this reactor to make just under 50g of MXene powder from 50g of MAX phase precursor material in about two days (including the time required for washing and drying the product). A battery of tests conducted by students at Drexel's Materials Science and Engineering Department showed that the reactor-produced MXene retains the morphology, and the electrochemical and physical properties, of the original lab-made substance.
This development puts MXenes in a group with just a handful of 2D materials that have proven they can be produced in industrial-size quantities. But because MXene-making is a subtractive manufacturing process – etching away bits of a raw material, like planing down lumber – it stands apart from the additive processes used to make many other 2D nanomaterials.
"Most 2D materials are made using a bottom-up approach," explained Christopher Shuck, a post-doctoral researcher in the A.J. Drexel Nanomaterials Institute. "This is where the atoms are added individually, one by one. These materials can be grown on specific surfaces or by depositing atoms using very expensive equipment. But even with these expensive machines and catalysts used, the production batches are time-consuming, small and still prohibitively expensive for widespread use beyond small electronic devices."
MXenes also benefit from a set of physical properties that should ease their path from processed material to final product – a hurdle that has tripped up some of today's widely used advanced materials.
"It typically takes quite a while to build out the technology and processing to get nanomaterials in an industrially usable form," Gogotsi said. "It's not just a matter of producing them in large quantities, it often requires inventing completely new machinery and processes to get them in a form that can be inserted into the manufacturing process – of a microchip or cell phone component, for example."
But for MXenes, integration into the manufacturing line should be fairly easy, according to Gogotsi.
"One huge benefit to MXenes is that they can be used as a powder right after synthesis or they can be dispersed in water, forming stable colloidal solutions," he said. "Water is the least expensive and the safest solvent. And with the process that we've developed, we can stamp or print tens of thousands of small and thin devices, such as supercapacitors or RFID tags, from material made in one batch."
This means the process can be applied to any of the standard variety of additive manufacturing systems – extrusion, printing, dip coating, spraying – after a single step of processing.
Several companies are already looking at developing applications for MXene materials, including Murata Manufacturing Co, Ltd., an electronics component company based in Kyoto, Japan, which is developing MXene technology for use in several high-tech applications.
"The most exciting part about this process is that there is fundamentally no limiting factor to an industrial scale-up," Gogotsi said. "There are more and more companies producing MAX phases in large batches, and a number of those are made using abundant precursor materials. And MXenes are among very few 2D materials that can be produced by wet chemical synthesis at large scale using conventional reaction engineering equipment and designs."
This story is adapted from material from Drexel University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.