Like a lead actress on the red carpet, nanowires—those superstars of nanotechnology—can be enhanced by a little jewelry, too. Not the diamonds and pearls variety, but the sort formed of sinuous chains of metal oxide or noble metal nanoparticles.
Though science has known for some time that such ornamentation can greatly increase the surface area and alter the surface chemistry of nanowires, engineers at Stanford University have found a novel and more effective method of “decorating” nanowires that is simpler and faster than previous techniques. The results of their study were published recently in the journal Nano Letters.
The development, say the researchers, might someday lead to better lithium-ion batteries, more efficient thin-film solar cells and improved catalysts that yield new synthetic fuels.
“You can think of it like a tree. The nanowires are the trunk, very good at transporting electrons, like sap, but limited in surface area,” explained Xiaolin Zheng, an assistant professor of mechanical engineering and senior author of the study. “The added nanoparticle decorations, as we call them, are like the branches and leaves, which fan out and greatly increase the surface area.” At the nanoscale, surface area matters a great deal in engineering applications like solar cells, batteries and, especially catalysts, where the catalytic activity is dependent on the availability of active sites at the surface of the material.
“Greater surface area means greater opportunity for reactions and therefore better catalytic capabilities in, for example, water-splitting systems that produce clean-burning hydrogen fuel from sunlight,” said Yunzhe Feng, a research assistant in Zheng’s lab and first author of the study. Other applications such as sensing small concentrations of chemicals in the air—of toxins or explosives, for example—might also benefit from the greater likelihood of detection made possible by increased surface area.
The key to the Stanford team’s discovery was a flame. Engineers had long known that nanoparticles could be adhered to nanowires to increase surface area, but the methods for creating them were not very effective in forming the much-desired porous nanoparticle chain structures. These other methods proved too slow and resulted in a too-dense, thick layer of nanoparticles coating the wires, doing little to increase the surface area.
Zheng and her team wondered whether a quick burst of flame might work better, so they tried it. Zheng dipped the nanowires in a solvent-based gel of metal and salt, then air-dried them before applying the flame. In her process the solvent burns away in a few seconds, allowing the all-important nanoparticles to crystalize into branch-like structures fanning out from the nanowires. “We were a little surprised by how well it worked,” said Zheng. “It performed beautifully.”
“It created these intricate, hair-like tendrils filled with lots of nooks and crannies,” said Zheng. "The bejeweled nanowires look like pipe cleaners. The resulting structure increases the surface many fold over what went before," she said.
Zheng and team have dubbed the technique the sol-flame method, for the combination of solvent and flame that yields the nanoparticle structures. The method appears general enough to work with many nanowire and nanoparticle materials and, perhaps more importantly, provides an unprecedented degree of engineering control in creating the nanoparticle decorations.
The high temperature of the flame and brief annealing time ensure that the nanoparticles are small and spread evenly across the nanowires. And, by varying the concentration of nanoparticle in the precursor solution and the number of times the wires are dip-coated, the Stanford team was able to vary the size of the nanoparticle decorations from tens to hundreds of nanometers, and the density from tens to hundreds of particles per square micrometer.
“Though more research is needed, such precision is crucial and could bolster the wider adoption of the process,” said Zheng.
By Andrew Myers
This story is reprinted from material from Stanford University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.