A microscope image of the novel oxide-based nanolattice. Image: The University of Texas at Austin/North Carolina State University.
A microscope image of the novel oxide-based nanolattice. Image: The University of Texas at Austin/North Carolina State University.

Researchers at the University of Texas (UT) at Austin and North Carolina (NC) State University have discovered, for the first time, a unique property in complex nanostructures that has thus far only been found in simple nanostructures. In addition, they have unraveled the internal mechanics of the materials that makes this property possible.

The researchers found this property in oxide-based ‘nanolattices’, which are tiny, hollow materials, akin to things like sea sponges in structure. They report their findings in a paper in the Proceedings of the National Academy of Sciences.

The property in question is called anelasticity, which relates to how materials react to stresses over time. When these novel nanolattices are bent, tiny defects move slowly in response to the stress gradient. When the stress is released, the tiny defects slowly return to their initial positions, resulting in the anelastic behavior.

"This has been seen before in simple nanostructures, like a nanowire, which is about 1000 times thinner than a hair," said Yong Zhu, a professor in the Department of Mechanical and Aerospace Engineering at NC State, and one of the lead authors of the paper. "But this is the first time we've seen it in a 3D nanostructure."

The researchers also discovered that when these defects move back and forth, they unlock energy dissipation characteristics, allowing them to dissipate things like pressure waves and vibrations.

This all means the nanolattice could someday serve as a shock absorber; but because the material is so lightweight and thin, this shock absorber would be on a very small scale. The researchers say it could find use in chips for electronics or other integrated electronic devices.

"You could potentially put this material under the semiconductor chips and protect them from outside impact or vibration," said Chih-Hao Chang, an associate professor in the Walker Department of Mechanical Engineering at UT Austin.

Now that these anelastic characteristics have been discovered, the next step is to control them. The researchers will examine the geometry of the nanostructures and experiment with different loading conditions to see how to optimize the anelastic performance for energy dissipation applications.

This story is adapted from material from the University of Texas at Austin, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.