This photo shows nanotube assemblies being drawn to the source of a Tesla field in an experiment at Rice University. Photo: Jeff Fitlow/Rice University.Scientists at Rice University, led by chemist Paul Cherukuri, have discovered that the strong force-field emitted by a Tesla coil causes carbon nanotubes to self-assemble into long wires, a phenomenon they call ‘Teslaphoresis’. Cherukuri sees this research, which is reported in ACS Nano, as setting a clear path toward scalable assembly of nanotubes from the bottom up.
Teslaphoresis works by remotely oscillating positive and negative charges in each nanotube, causing them to chain together into long wires. Cherukuri's specially-designed Tesla coil even generates a tractor beam-like effect to pull the nanotube wires toward the coil over long distances.
According to Cherukuri, this force-field effect on matter had never been observed before on such a large scale, and the phenomenon was unknown to Nikola Tesla, who invented the coil in 1891 with the intention of delivering wireless electrical energy. "Electric fields have been used to move small objects, but only over ultrashort distances," Cherukuri said. "With Teslaphoresis, we have the ability to massively scale up force-fields to move matter remotely."
The researchers discovered that the phenomenon simultaneously assembles and powers circuits that can harvest energy from the wider environment. In one experiment, nanotubes assembled themselves into wires, formed a circuit connecting two LEDs and then absorbed sufficient energy from the Tesla coil's field to light them up.
Cherukuri realized that a redesigned Tesla coil could create a powerful force-field at distances far greater than anyone imagined. His team observed alignment and movement of the nanotubes several feet away from the coil. "It is such a stunning thing to watch these nanotubes come alive and stitch themselves into wires on the other side of the room," he said.
Nanotubes were a natural first test material, given their heritage at Rice, where the HiPco production process was invented. But the researchers envision that Teslaphoresis could be used to self-assemble many other nanomaterials as well.
Lindsey Bornhoeft, the paper's lead author and a biomedical engineering graduate student at Texas A&M University, said the directed force-field from the bench-top coil at Rice is restricted to just a few feet. To examine the effects on matter at greater distances would require larger systems that are under development. Cherukuri suggested that patterned surfaces and multiple Tesla coil systems might be able to create more complex self-assembling circuits from nanoscale-sized particles.
Cherukuri and his wife, Tonya, also a Rice alumnus and a co-author of the paper, noted that their son Adam made some remarkable observations while watching videos of the experiment. "I was surprised that he noticed patterns in nanotube movements that I didn't see," Cherukuri said. "I couldn't make him an author on the paper, but both he and his little brother John are acknowledged for helpful discussions."
Cherukuri knows the value of youthful observation and imagination, as he started designing Tesla coils as a teen. "I would have never thought, as a 14-year-old kid building coils, that it was going to be useful someday," he said.
Cherukuri and his team self-funded this work, which he said made it more meaningful for the group. "This was one of the most exciting projects I've ever done, made even more so because it was an all-volunteer group of passionate scientists and students. But because Rice has this wonderful culture of unconventional wisdom, we were able to make an amazing discovery that pushes the frontiers of nanoscience."
The teammates look forward to seeing where their research now leads. "These nanotube wires grow and act like nerves, and controlled assembly of nanomaterials from the bottom up may be used as a template for applications in regenerative medicine," Bornhoeft said.
"There are so many applications where one could utilize strong force fields to control the behavior of matter in both biological and artificial systems," Cherukuri said. "And even more exciting is how much fundamental physics and chemistry we are discovering as we move along. This really is just the first act in an amazing story."
This story is adapted from material from Rice University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.