(Left) Top and side views of the crystal structures of perovskite-derived Cs3Bi2I9, a material synthesized at Rice University that shows valleytronics capabilities. Each unit cell contains two neighboring layers with a weak van der Waals interaction in between. (Right) An image showing triangles of the material on a mica substrate. Image: Lou Group/Rice University.Engineers at Rice University and Texas A&M University have found a 2D material that could make computers faster and more energy-efficient. Their material is a derivative of perovskite – a crystal with a distinctive structure – that shows a surprising potential for use in valleytronics, which is being touted as a possible novel platform for information processing and storage.
The lab of materials scientist Jun Lou at Rice's Brown School of Engineering synthesized a layered material of cesium, bismuth and iodine (Cs3Bi2I9) that is adept at storing the valley states of electrons, but only in the material's odd layers. According to Lou and his colleagues, not only can these valley states can be set with polarized light, but the material's even layers appear to protect the odd layers from the kind of field interference that bedevils other perovskites. Best of all, the material appears to be scalable.
"This is not a new material, but we figured out a way to make it without solution processing or exfoliating it from bulk," Lou said. "What's novel is that we can produce it (via chemical vapor deposition) in a few layers, and all the way down to a monolayer. That enabled us to probe its nonlinear optical properties." The engineers report their work in a paper in Advanced Materials.
Valleytronics is a cousin to spintronics, in which memory bits are defined by an electron's quantum spin state. In valleytronics, electrons have degrees of freedom in the multiple momentum states – or valleys – they occupy. These states can be read as bits.
"In a transistor, if you put an electron there, it represents a state, and if you take it out, that represents another state," explained co-principal investigator Hanyu Zhu of Rice University. "In valleytronics, the electrons are always present, and are in either of two different quantum wavefunctions with opposite momenta. These two wavefunctions interact with different light polarization, so the momentum state can be resolved optically."
A close look at the inorganic, layered material with an electron microscope showed that molecules in the odd layer are asymmetric. "That lack of symmetry is missing in the even layers – that's how we differentiate between them – and it gives rise to the properties we see," Lou said. "That's just the nature of this crystal structure."
The lab tested versions of the material with up to 11 layers and found that a lack of transparency didn't seem to affect how well light could trigger a response. "Even a thicker material behaves like it's still a single layer," Lou said. "That's quite important."
"Thicker 2D transition metal dichalcogenides lose unique properties like valleytronics. All the behaviors are gone. That's not the case for this material."
Calculations by co-principal investigator Xiaofeng Qian of Texas A&M University provided the necessary theoretical evidence. "The valley polarization observed in both thin and thick layers is largely due to the weak interlayer electronic coupling, a unique feature of this perovskite derivative compared to other 2D materials when stacked together," Qian said. "It also leads to persistent nonlinear optical responses in thicker samples."
The material also seems less susceptible to environmental degradation, a common problem for hybrid perovskites developed for solar energy. "This material won't give you very high conversion efficiency, but think of it like an all-around athlete in the Olympic Games," said lead author and Rice postdoctoral fellow Jia Liang. "It may not be the best in each category, but if you consider its different aspects together, it will stand out."
The researchers suggested that the already strong light-matter interaction they observed could be enhanced by further engineering the material's band gap. "I think it's a breakthrough for using this type of material in information processing," Lou said. "We're really hoping this is the starting point."
This story is adapted from material from Rice University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.