Rice University postdoctoral researcher Yilin Li holds up a glowing windowpane with a conjugated polymer center that serves as a waveguide, sending certain frequencies of light to the edges of the pane, where they can be absorbed by solar cells. Photo: Yilin Li/Rice University.Engineers at Rice University have suggested a colorful solution to next-generation energy collection: windows with luminescent solar concentrators (LSCs). Led by Rafael Verduzco and postdoctoral researcher Yilin Li at Rice's Brown School of Engineering, the team designed and built foot-square 'windows' that sandwich a conjugated polymer between two clear acrylic panels.
The thin middle layer is the secret sauce: it's designed to absorb light of a specific wavelength and guide it to panel edges lined with solar cells. Conjugated polymers are chemical compounds that can be tuned to possess specific chemical or physical properties for a variety of applications, like conductive films or sensors for biomedical devices.
The Rice lab's polymer compound is called PNV (poly[naphthalene-alt-vinylene]). It absorbs and emits red light, but adjusting the molecular ingredients should make it able to absorb light in a variety of colors. The trick is that, as a waveguide, it accepts light from any direction but restricts how it leaves, concentrating the light onto solar cells at the panel edges that convert it to electricity.
"The motivation for this research is to solve energy issues for buildings through integrated photovoltaics," said Li, who began the project as part of a 'smart glass' competition. "Right now, solar rooftops are the mainstream solution, but you need to orient them toward the Sun to maximize their efficiency, and their appearance isn't very pleasing.
"We thought, why can't we make colorful, transparent or translucent solar collectors and apply them to the outside of buildings?" The engineers report their work in a paper in Polymer International.
Admittedly, the amount of juice generated by the Rice team's test units is far less than that collected by even average commercial solar cells, which routinely convert about 20% of sunlight into electricity.
But LSC windows never stop working. They happily recycle light from inside the building into electricity when the Sun goes down. In fact, tests showed they were actually more efficient at converting ambient light from LEDs than direct sunlight, even though the sunlight was 100 times stronger.
"Even indoors, if you hold up a panel, you can see very strong photoluminescence on the edge," Li said. The panels he tested showed a power conversion efficiency of up to 2.9% in direct sunlight and 3.6% under ambient LED light.
Various types of luminophores have been developed over the past decade, but rarely with conjugated polymers.
"Part of the problem with using conjugated polymers for this application is that they can be unstable and degrade quickly," said Verduzco, a professor of chemical and biomolecular engineering and of materials science and nanoengineering. "But we've learned a lot about improving the stability of conjugated polymers in recent years, and in the future, we can engineer the polymers for both stability and desired optical properties."
The lab also simulated the return of energy from panels as large as 120 inches square. They reported that these panels would provide somewhat less energy, but it would still contribute to a household's needs.
Li noted that the polymer might also be tuned to convert energy from infrared and ultraviolet light, allowing the panels to remain transparent. "The polymers can even be printed in patterns in the panels, so they can be turned into artwork," he said.
This story is adapted from material from Rice University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.