Upon illumination with red light, third harmonic scattered light (in violet) reveals the twist of metal nanoparticles. Photo: Ventsislav Valev and Lukas Ohnoutek.Physics researchers at the University of Bath in the UK have discovered a new physical effect relating to the interaction between light and twisted materials – an effect that is likely to have implications for emerging new nanotechnologies in communications, nanorobotics and ultra-thin optical components. They report their findings in a paper in Laser & Photonics Reviews.
In the 17th and 18th centuries, the Italian master craftsman Antonio Stradivari produced musical instruments of legendary quality, and most famous are his (so-called) Stradivarius violins. What makes the musical output of these musical instruments both beautiful and unique is their particular timbre, also known as tone color or tone quality. All instruments have a timbre – when a musical note (sound with frequency fs) is played, the instrument creates harmonics (frequencies that are an integer multiple of the initial frequency, i.e. 2fs, 3fs, 4fs, 5fs, 6fs, etc).
Similarly, when light of a certain color (with frequency fc) shines on materials, these materials can produce harmonics (light frequencies 2fc, 3fc, 4fc, 5fc, 6fc, etc). The harmonics of light can reveal intricate material properties that find applications in medical imaging, communications and laser technology.
For example, virtually every green laser pointer is in fact an infrared laser pointer whose light is invisible to human eyes. The green light that we see is actually the second harmonic (2fc) of the infrared laser pointer and it is produced by a special crystal inside the pointer.
In both musical instruments and shiny materials, some frequencies are ‘forbidden’ – that is, they cannot be heard or seen because the instrument or material actively cancels them. Because the clarinet has a straight, cylindrical shape, it supresses all of the even harmonics (2fs, 4fs, 6fs, etc) and produces only odd harmonics (3fs, 5fs, 7fs, etc). By contrast, a saxophone has a conical and curved shape that allows all harmonics and results in a richer, smoother sound.
Somewhat similarly, when a specific type of light (circularly polarised) shines on metal nanoparticles dispersed in a liquid, the odd harmonics of light cannot propagate along the direction of light travel and the corresponding colors are forbidden.
Now, an international team of scientists led by researchers from the Department of Physics at the University of Bath has found a way to reveal the forbidden colors, amounting to the discovery of a new physical effect. To achieve this result, they ‘curved’ their experimental equipment.
“The idea that the twist of nanoparticles or molecules could be revealed through even harmonics of light was first formulated over 42 years ago, by a young PhD student – David Andrews," explained Ventsislav Valev at the University of Bath, who led the research. "David thought his theory was too elusive to ever be validated experimentally but, two years ago, we demonstrated this phenomenon. Now, we discovered that the twist of nanoparticles can be observed in the odd harmonics of light as well. It’s especially gratifying that the relevant theory was provided by none other than our co-author and nowadays well-established professor – David Andrews!
“To take a musical analogy, until now, scientists who study twisted molecules (DNA, amino acids, proteins, sugars, etc) and nanoparticles in water – the element of life – have illuminated them at a given frequency and have either observed that same frequency or its noise (inharmonic partial overtones). Our study opens up the study of the harmonic signatures of these twisted molecules. So, we can appreciate their ‘timbre’ for the first time.
“From a practical point of view, our results offer a straightforward, user-friendly experimental method to achieve an unprecedented understanding of the interactions between light and twisted materials. Such interactions are at the heart of emerging new nanotechnologies in communications, nanorobotics and ultra-thin optical components. For instance, the ‘twist’ of nanoparticles can determine the value of information bits (for left-handed or right-handed twist). It is also present in the propellers for nanorobots and can affect the direction of propagation for a laser beam. Moreover, our method is applicable in tiny volumes of illumination, suitable for the analysis of natural chemical products that are promising for new pharmaceuticals but where the available material is often scarce.”
“We came very close to missing this discovery," said Bath PhD student Lukas Ohnoutek, who was also involved in the research. "Our initial equipment was not ‘tuned’ well and so we kept seeing nothing at the third-harmonic. I was starting to lose hope, but we had a meeting, identified potential issues and investigated them systematically until we discovered the problem. It is wonderful to experience the scientific method at work, especially when it leads to a scientific discovery!”
‘‘Professor Valev has led an international team to a real first in the applied photonics," added Andrews. "When he invited my participation, it led me back to theory work from my doctoral studies. It has been amazing to see it come to fruition so many years later.”
This story is adapted from material from the University of Bath, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.