The new aerogel insulating material is highly transparent, transmitting 95% of light. In this photo, parallel laser beams are used to make the material visible. Photo: Lin Zhao.
The new aerogel insulating material is highly transparent, transmitting 95% of light. In this photo, parallel laser beams are used to make the material visible. Photo: Lin Zhao.

A newly developed material that is so transparent you can barely see it could unlock many new uses for solar heat. It generates much higher temperatures than conventional solar collectors – enough to be used for home heating or for industrial processes that require heat of more than 200°C (392°F).

The key to the process is a new kind of aerogel, a lightweight material that consists mostly of air, with a structure made of silica (which is also used to make glass). The material, which was developed by researchers at Massachusetts Institute of Technology (MIT), lets sunlight pass through easily but blocks solar heat from escaping. The researchers report the material in a paper in ACS Nano.

The key to efficient collection of solar heat, explains Evelyn Wang, professor and head of the Department of Mechanical Engineering, is being able to keep something hot internally while remaining cold on the outside. One way of doing that is by establishing a vacuum between a layer of glass and a dark, solar-absorbing material. This setup is used in many concentrating solar collectors, but it's relatively expensive to install and maintain. There has been great interest in finding a less expensive, passive system for collecting solar heat at the high temperature levels needed for space heating, food processing and many industrial processes.

Aerogels, a kind of foam-like material made of silica particles, have been developed for years as highly efficient and lightweight thermal insulating materials, but they have generally had limited transparency to visible light, with a transmission level of around 70%. Wang says making aerogels that are transparent enough to work for solar heat collection was a long and difficult process involving several researchers for about four years. But the result is an aerogel that lets through over 95% of incoming sunlight while maintaining the material's highly insulating properties.

The key is in the precise ratios of the different chemicals used to create the aerogel, which is made by mixing a catalyst with a silicon-containing compound in a liquid solution to form a kind of wet gel and then drying it to get all the liquid out. This leaves a matrix that is mostly air but retains the original mixture's structure. The researchers found that producing a mix that chemically reacts much more quickly than in conventional aerogels resulted in a gel with smaller pore spaces between its grains, meaning it scattered light much less.

In tests on a rooftop on the MIT campus, a passive device consisting of a solar-absorbing dark material covered with a layer of the new aerogel was able to reach and maintain a temperature of 220°C, in the middle of a Cambridge winter when the outside air was below 0°C.

Such high temperatures have previously only been obtained with concentrating systems, which use mirrors to focus sunlight onto a central line or point, but the new system requires no concentration, making it simpler and less costly. That could potentially make it useful for a wide variety of applications that require higher levels of heat.

For example, simple flat rooftop collectors are often used for domestic hot water, producing temperatures of around 80°C. But the higher temperatures generated by the aerogel could make such simple systems usable for home heating, while large-scale versions could be used to provide heat for a wide variety of applications in chemical, food production and manufacturing processes.

Zhao describes the basic function of the aerogel layer as "like a greenhouse effect. The material we use to increase the temperature acts like the Earth's atmosphere does to provide insulation, but this is an extreme example of it."

For most purposes, the passive heat collection system would need to be connected to pipes containing a liquid that could circulate, in order to transfer the heat to wherever it's needed. Alternatively, Wang suggests, for some uses the system could be connected to heat pipes, devices that can transfer heat over a distance without requiring pumps or any moving parts.

Because the principle is essentially the same, an aerogel-based solar heat collector could directly replace the vacuum-based collectors used in some existing applications, providing a lower-cost option. The materials used to make the aerogel are all abundant and inexpensive. The only costly part of the process is the drying, which requires a specialized device called a critical point dryer. This employs a very precise drying process to extract the solvents from the gel while preserving its nanoscale structure.

Because that is a batch process, rather than a continuous one that can be used in roll-to-roll manufacturing, it could limit the rate of production if the system is scaled up to industrial production levels. "The key to scaleup is how we can reduce the cost of that process," Wang says. But even now, a preliminary economic analysis shows that the system can be economically viable for some uses, especially in comparison with vacuum-based systems.

This story is adapted from material from MIT, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.