This series of images shows how a new retroreflective material can be used to make a color-changing speed limit sign. Boxes A-F show how the sign changes color from the perspective of drivers on the road as they pass by. Image: Fan et al., Sci. Adv. 2019; 5 : eaaw8755.
This series of images shows how a new retroreflective material can be used to make a color-changing speed limit sign. Boxes A-F show how the sign changes color from the perspective of drivers on the road as they pass by. Image: Fan et al., Sci. Adv. 2019; 5 : eaaw8755.

A thin film that reflects light in intriguing ways could be used to make road signs that shine brightly and change color at night, according to a study reported in a paper in Science Advances. This new technology could help call attention to important traffic information when it's dark, with potential benefits for both drivers and pedestrians, researchers say.

The film consists of polymer microspheres laid down on the sticky side of a transparent tape. The material's physical structure leads to an interesting phenomenon: when white light shines on the film at night, some observers will see a single, stable color reflected back, while others will see changing colors. It all depends on the angle of observation and whether the light source is moving.

The research was led by Limin Wu at Fudan University in China, whose group developed the material. Experts on optics at the University at Buffalo (UB) also made significant contributions to the work, by providing insight into potential applications for the film, such as employing it in night-time road signs.

"You can use this material to make smart traffic signs," says Qiaoqiang Gan, an associate professor of electrical engineering in the UB School of Engineering and Applied Sciences and a co-first author of the paper. "If a person is listening to loud music or isn't paying attention while they're walking or driving, a color-changing sign can help to better alert them to the traffic situation."

In one set of experiments, the researchers created a speed limit sign with letters and numbers made from the new film. They placed a white light nearby to illuminate the sign, and when a fast-moving car drove past, the driver saw the color of the characters on the sign appear to flicker as their viewing angle changed.

In other tests, the team applied the new material to a series of markers lining the side of a road, denoting the boundary of the driving lane. As a car approached, the markers lit up in bright colors, reflecting light from the vehicle's headlights.

From the driver's perspective, the markers' color remained stable. But to a pedestrian standing at the side of the road, the color of the markers appeared to flicker as the car and its headlights sped past.

"If the car goes faster, the pedestrian will see the color change more quickly, so the sign tells you a lot about what is going on," says co-author Haomin Song, UB assistant professor of research in electrical engineering.

This story is adapted from material from the University at Buffalo, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.