Researchers at Purdue University have created a new formula for the world's whitest paint, making it thinner and lighter. The previous iteration (left) required a layer 0.4mm thick to achieve sub-ambient radiant cooling. The new formulation (right) can achieve similar cooling with a layer just 0.15mm thick. Image: Purdue University photo/Andrea Felicelli.The world’s whitest paint keeps surfaces so cool that it could reduce the need for air conditioning (see Cool paint shows white is the new black). Now the Purdue University researchers who created the paint have developed a new formulation that is thinner and lighter – ideal for radiating heat away from cars, trains and airplanes.
“I’ve been contacted by everyone from spacecraft manufacturers to architects to companies that make clothes and shoes,” said Xiulin Ruan, a professor of mechanical engineering at Purdue University and developer of the paint. “They mostly had two questions: where can I buy it, and can you make it thinner?”
The original world’s whitest paint used nanoparticles of barium sulfate to reflect 98.1% of sunlight, thus cooling outdoor surfaces more than 4.5°C below ambient temperature. Cover your roof in that paint, and you could essentially cool your home with much less air conditioning. But there’s a catch.
“To achieve this level of radiative cooling below the ambient temperature, we had to apply a layer of paint at least 400µm thick,” Ruan said. “That’s fine if you’re painting a robust stationary structure, like the roof of a building. But in applications that have precise size and weight requirements, the paint needs to be thinner and lighter.”
That’s why Ruan’s team began experimenting with other materials, pushing the limit of their capability to scatter sunlight. Their latest formulation is a nanoporous paint incorporating hexagonal boron nitride as the pigment, a substance mostly used in lubricants. This new paint achieves nearly the same benchmark of solar reflectance (97.9%) but with just a single 150µm-layer of paint. Ruan and his team report their advance in a paper in Cell Reports Physical Science.
“Hexagonal boron nitride has a high refractive index, which leads to strong scattering of sunlight,” said Andrea Felicelli, a Purdue PhD student in mechanical engineering who worked on the project. “The particles of this material also have a unique morphology, which we call nanoplatelets.”
Ioanna Katsamba, another PhD student in mechanical engineering at Purdue, ran computer simulations to understand if the nanoplatelet morphology offers any benefits. “The models showed us that the nanoplatelets are more effective in bouncing back the solar radiation than spherical nanoparticles used in previous cooling paints,” Katsamba said.
The paint also incorporates voids of air, which make it highly porous at the nanoscale. This lower density, together with the thinness, provides another huge benefit – reduced weight. The newer paint weighs 80% less than barium sulfate paint, yet achieves nearly identical solar reflectance.
“This light weight opens the doors to all kinds of applications,” said George Chiu, a Purdue professor of mechanical engineering and an expert in inkjet printing. “Now this paint has the potential to cool the exteriors of airplanes, cars or trains. An airplane sitting on the tarmac on a hot summer day won’t have to run its air conditioning as hard to cool the inside, saving large amounts of energy. Spacecraft also have to be as light as possible, and this paint can be a part of that.”
As to that other big question – where can I buy the paint? – Ruan explains: “We are in discussions right now to commercialize it. There are still a few issues that need to be addressed, but progress is being made.”
Either way, the Purdue researchers look forward to what the paint could accomplish. “Using this paint will help cool surfaces and greatly reduce the need for air conditioning,” Ruan said. “This not only saves money, but it reduces energy usage, which in turn reduces greenhouse gas emissions. And unlike other cooling methods, this paint radiates all the heat into deep space, which also directly cools down our planet. It’s pretty amazing that a paint can do all that.”
This story is adapted from material from Purdue University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.