"We are trying to make a gel that you could inject with a pin, and then you'd have a little blob that would dissolve away very slowly for three to six months to provide continuous therapy. This would be a game-changer for fighting critical diseases around the world."Eric Appel, Stanford University
Gels are formed by mixing polymers into fluids to create gooey substances useful for everything from holding hair in place to enabling contact lenses to float over the eye.
Researchers want to develop gels for healthcare applications by mixing in medicinal compounds and giving patients injections so that the gel releases the active pharmaceutical ingredient over a period of months to avoid weekly or daily needle pricks. But standing in the way is a problem that's as easily understandable as the difference between using hair gel on a beach versus in a blizzard – heat and cold change the character of the gel.
"We can make gels with the right slow-release properties at room temperature, but once we injected them body heat would rapidly dissolve them and release the medicines too quickly," said Eric Appel, assistant professor of materials science and engineering at Stanford University.
In a paper in Nature Communications, Appel and his team detail their successful first step toward making temperature-resistant, injectable gels with a concoction designed to cleverly bend the laws of thermodynamics.
Appel explained the science behind this rule-breaking with an analogy to making Jello. The solid Jello ingredients are first poured into water, then heated and stirred to mix well. As the mixture cools, the Jello solidifies as the molecules bond together. But if the Jello is reheated, the solid reliquefies.
The Jello example illustrates the interplay between two thermodynamic concepts – enthalpy, which measures the energy added to or subtracted from a material, and entropy, which describes how energy changes make a material more or less orderly at the molecular level. Appel and his team had to make a medicinal Jello that didn't melt, thus losing its time-release properties, when the cool solid was heated by the body.
To accomplish this, the Stanford team created a gel made of two solid ingredients – polymers and nanoparticles. The polymers were long, spaghetti-like strands with a natural propensity to get entangled, while the nanoparticles encouraged this propensity.
The researchers began by separately dissolving the polymers and nanoparticles in water and then stirring them together. As the commingling ingredients began to bond, the polymers wrapped tightly around the particles. "We call this our molecular Velcro," said first author Anthony Yu, who did the work as a Stanford graduate student and is now a postdoctoral scholar at Massachusetts Institute of Technology.
The powerful affinity between the polymers and nanoparticles squeezed out the water molecules that had been caught between them, and as more polymers and particles congealed, the mixture began to gel at room temperature. Crucially, this gelling process was achieved without adding or subtracting energy. When the researchers exposed this gel to the body's temperature (37.5°C), they found it didn't liquefy like ordinary gels because the molecular Velcro effect allowed entropy and enthalpy – orderliness and temperature change, respectively – to remain roughly in balance in accordance with thermodynamics.
Appel said it will take more work to make injectable, time-release gels that are safe for human use. While the polymers in these experiments were biocompatible, the particles were derived from polystyrene, which is commonly used to make disposable cutlery. His lab is already trying to make thermodynamically neutral gels with fully biocompatible components.
If they are successful, a time-release gel could prove valuable for providing anti-malarial or anti-HIV treatments in under-resourced areas where it's difficult to administer the short-acting remedies currently available.
"We are trying to make a gel that you could inject with a pin, and then you'd have a little blob that would dissolve away very slowly for three to six months to provide continuous therapy," Appel said. "This would be a game-changer for fighting critical diseases around the world."
This story is adapted from material from Stanford University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.