Researchers at North Carolina State University have created 3D-printed, flexible mesh structures that can be controlled with applied magnetic fields while floating on water. The structures can grab small objects and carry water droplets, which means they could potentially act as soft robots that can mimic creatures living on water surfaces or serve as tissue scaffolds for cell cultures.
"This research shows capabilities in the emerging field of combining 3D printing and soft robotics," said Orlin Velev, professor of chemical and biomolecular engineering at NC State and corresponding author of a paper in Advanced Materials Technologies describing the research.
To create these structures, the researchers made an ‘ink’ from silicone microbeads, bound by liquid silicone and contained in water. The resulting ‘homocomposite thixotropic paste’ resembles common toothpaste, which can easily be squeezed out of a tube but then maintains its shape on your toothbrush without dripping.
The researchers used a 3D printer to shape this paste into mesh-like patterns. The patterns are then cured in an oven to create flexible silicone structures that can be controlled – stretched and collapsed – by the application of magnetic fields.
"This self-reinforced paste allows us to create structures that are ultra-soft and flexible," said Sangchul Roh, an NC State PhD student in Velev's lab and first author of the paper.
"Embedding of iron carbonyl particles, which are widely available and have a high magnetization, allows us to impart a strong response to magnetic field gradients," added Joseph Tracy, professor of materials science and engineering at NC State and a senior co-investigator on the project.
"The structures are also auxetic, which means that they can expand and contract in all directions," Velev said. "With 3D printing, we can control the shape before and after the application of the magnetic field."
The structures' properties also allow them to be used while floating on water, similar to water striders, or insects that skim or hop across water surfaces.
"Mimicking live tissues in the body is another possible application for these structures," Roh said.
In the paper, the researchers showed how they were able to design reconfigurable meshes, including a structure that could ‘grab’ a tiny ball of aluminum foil and a structure that could ‘carry’ a single water droplet and then release it on demand through the mesh. "For now, this is an early stage proof-of-concept for a soft robotic actuator," Velev said.
This story is adapted from material from North Carolina State University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.