Cookies enable us to provide the best experience possible and help us understand how visitors use our website. By browsing Materials Today, you agree to our use of cookies.
The EPMA says that its next Euro PM Congress & Exhibition will take place in Lisbon, Portugal, from 4–7 October 2020.
Höganäs says that its new atomizing plant has received building approval by the local council.
The Powder Coating Institute (PCI) has published the program for the Powder Coating Week 2020, taking place from 17–20 February in Orlando, FL, USA.
Siemens and Materials Solutions, a Siemens business, have opened an innovation center in Orlando, Florida.
Equispheres says that in tests its metal powders allowed for a 50% increase in production speeds and a 20-30% increase in a-basis mechanical performance.
Standards developer ASTM International has announced a second round of funding to support additive manufacturing (AM) standards research.
The EPMA says that it will hold a meeting to discuss implementing a project focused on analysing PM mechanical behavior and microstructures.
The EPMA says that a newly updated Euro PM2019 Congress and Exhibition technical program is now online.