Biomaterials are typically chosen for their chemical inertness and low surface energies. However, these properties can also make it difficult to effectively apply functional coatings and facilitate desirable interactions with other surfaces. This article discusses the benefits of plasma treating biomaterials in order to further enhance their functionality as well as gives example applications and plasma treatment processing guidelines.