A water droplet bounces off a hydrophobic coating on a surface that has been burned and abraded. Photo: Joseph Xu/Multimedia Content Producer, University of Michigan – College of Engineering.A self-healing, water-repellent, spray-on coating developed at the University of Michigan (U-M) is hundreds of times more durable than its counterparts.
This novel coating could be used to waterproof vehicles, clothing, rooftops and countless other surfaces exposed to conditions that are too harsh for current waterproofing treatments. It could also lower the resistance of ship hulls, a step that would reduce the fuel consumption of the massive vessels that transport 90% of the world's cargo.
The developers say the new concoction is a breakthrough in a field where decades of research have failed to produce a durable coating. While water-repellent finishes are available at present, they're typically not strong enough for applications like clothing or ship hulls. This discovery changes that.
"Thousands of superhydrophobic surfaces have been looked at over the past 20 or 30 years, but nobody has been able to figure out how to systematically design one that's durable," said Anish Tuteja, U-M associate professor of materials science and engineering. "I think that's what we've really accomplished here, and it's going to open the door for other researchers to create cheaper, perhaps even better superhydrophobic coatings."
The novel coating is made of a mix of a material called ‘fluorinated polyurethane elastomer’ and a specialized water-repellent molecule known as ‘F-POSS’. It can be easily sprayed onto virtually any surface and has a slightly rubbery texture that makes it more resilient than its predecessors.
If it is damaged, the coating can heal itself hundreds of times. It can bounce back "even after being abraded, scratched, burned, plasma-cleaned, flattened, sonicated and chemically attacked," the researchers write in a paper in ACS Applied Materials & Interfaces.
In addition to recovering physically, the coating can heal itself chemically. If water-repellent F-POSS molecules are scraped from the surface, new molecules will naturally migrate there to replace them. That's how the coating can renew itself hundreds of times; its healing ability is limited only by its thickness.
The coating is already being commercialized by HygraTek, a company founded by Tuteja, with assistance from U-M Tech Transfer. Beyond the coatings detailed in the paper, this project also produced what amounts to a recipe that researchers can use to optimize future coatings for a specific application's requirements in terms of cost, durability and other factors.
As lead author and U-M doctoral student Kevin Golovin explains, the team used a process that was radically different from previous research in the field. "Most materials science researchers have focused on identifying one specific chemical system that's as durable and water-repellent as possible," he said. "We approached the problem differently, by measuring and mapping out the basic chemical properties that make a water-repellent coating durable. And some of the results surprised us."
For example, most hydrophobic coatings are made of two main ingredients: an active molecule that provides the water-repellency and a binder. Generally, researchers have assumed that using more durable ingredients would make a more durable coating. But Tuteja's team found that's not necessarily the case.
They discovered that even more important than durability is a property called ‘partial miscibility’, or the ability of two substances to partially mix together. The other key variable the team discovered is the stability of the water-repellent surface.
Most water-repellent coatings work because their surface has a very specific geometry, often microscopic pillars. Water droplets perch on top of these pillars, creating air pockets underneath that deny the water a solid place to rest and cause it to roll off easily. But such surfaces tend to be fragile – slight abrasion or even the pressure of the water itself can damage them.
The team's research revealed that a slightly pliable surface can escape this pitfall – even though it seems less durable, its pliable properties allow it to bounce back from damage.
Tuteja estimates that the coatings will be available for use before the end of 2017 for applications including water-repellent fabrics and spray-on coatings that can be purchased directly by consumers.
This story is adapted from material from the University of Michigan, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.