By using a novel X-ray technique, researchers have observed a catalyst surface at work in real time and were able to resolve its atomic structure in detail. The new technique, pioneered at DESY's X-ray light source PETRA III, may pave the way for the design of better catalysts and other materials on the atomic level. It greatly speeds up the determination of atomic surface structures and enables live recordings of surface reactions like catalysis, corrosion and growth processes with a time resolution of less than a second. “We can now investigate surface processes that were not observable in real time before and that play a central role in many fields of materials science,” explains DESY researcher Prof. Andreas Stierle. The Swedish-German research team around lead author Dr. Johan Gustafson of Lund University present their work in the US journal Science.
Materials scientists currently lack a method to record data of the full atomic structure of surfaces during dynamic processes within a reasonable time. Existing methods are either too slow or require ultra high vacuum, prohibiting the flow of gas in the test chamber and thus ruling out a live investigation of dynamic reaction processes involving gas phases at near atmospheric pressures.
“Our goal was to observe surfaces under reactive, application-oriented conditions in real time,” says Stierle. The team used the high-energy X-rays from DESY's light source PETRA III. When X-rays strike a solid material, they are diffracted into a characteristic pattern that yields information about the atomic structure of the material. In conventional X-ray measurements performed at lower photon energies, the sample and the detector must be rotated to map out the full diffraction pattern painstakingly step by step, a procedure that can easily consume ten hours or more.
"This approach makes it possible to record data 10 to 100 times faster..."Professor Andreas Stierle, DESY researcher.
In contrast, the high-energy X-rays of PETRA III are scattered into a much smaller angular range, producing a much more compact diffraction pattern that can be recorded at once with a high-end two-dimensional detector at the High-Energy Materials Science measuring station P07. "This approach makes it possible to record data 10 to 100 times faster,” explains Stierle. As a consequence, scientists can gain a full surface structure in less than ten minutes or track individual structural features with a temporal resolution of less than a second. “It also allows us to more easily identify unknown or unexpected structures,” underlines Stierle.
For their investigations, the researchers installed a test chamber, in which the gas pressure can be up to 1 bar — the same as normal atmospheric pressure — to approach realistic reaction conditions. A mass spectrometer allows for on-line monitoring of the gas distribution within the test chamber during measurements.
To demonstrate the new approach, the researchers watched a catalyst of the precious metal palladium live at work: a two millimetre thick palladium single crystal with a diameter of one centimetre converts toxic carbon monoxide into harmless carbon dioxide, much like catalytic converters do in cars. The technique enabled the scientists to observe how the palladium began to convert the carbon monoxide (CO) into carbon dioxide (CO2) as soon as oxygen (O2) also flowed into the chamber. “We can watch how the catalyst switches from a non-reactive state into a reactive one,” explains Stierle who heads the NanoLab at DESY and also holds an appointment as professor at the University of Hamburg.
The researchers hope to identify the catalyst’s active phase by using this new approach. “The new technology gives us the opportunity to identify the reaction centres in real time at atomic resolution,” says Stierle.
In the end, the findings could be used to optimise catalysts.The new X-ray technique has a wide variety of applications for materials research. The scientists expect completely new insights into the kinetics of surface processes, enabling the design of new materials on the atomic level. “The combination of the extremely bright X-ray source, the sample environment and the 2D detector at PETRA III is worldwide unique,” emphasises Stierle.
This story is reprinted from material from DESY, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.