Organic solar cells now exceed 10% efficiency igniting interest not only in the fundamental molecular design of the photoactive semiconducting materials, but also in overlapping fields such as green chemistry, large-scale processing and thin film stability. For these devices to be commercially useful, they must have lifetimes in excess of 10 years. One source of potential instability, is that the two bicontinuous phases of electron donor and acceptor materials in the photoactive thin film bulk heterojunction, change in dimensions over time. Photocrosslinking of the p-conjugated semiconducting donor polymers allows the thin film morphology to be ‘locked’ affording patterned and stable blends with suppressed fullerene acceptor crystallization. This article reviews the performance of crosslinkable polymers, fullerenes and additives used to-date, identifying the most promising.