Nanowire-based one-dimensional electronics
Volume 9, Issue 10, Page 28–35
| C. Thelander, P. Agarwal, S. Brongersma, J. Eymery, L.F. Feiner, A. Forchel, M. Scheffler, W. Riess, B.J. Ohlsson, U. Gösele, L. Samuelson
During the last half century, a dramatic downscaling of electronics has taken place, a miniaturization that the industry expects to continue for at least a decade. We present efforts to use the self-assembly of one-dimensional semiconductor nanowires1 in order to bring new, high-performance nanowire devices as an add-on to mainstream Si technology. The nanowire approach offers a coaxial gate-dielectric-channel geometry that is ideal for further downscaling and electrostatic control, as well as heterostructure-based devices on Si wafers.