The paper presents a method on how the mean stress effect on fatigue damage can be taken into account under an arbitrary low cycle thermo-mechanical loading. From known stress, elastoplastic strain and temperature histories the cycle amplitudes and cycle mean values are extracted and the damage parameter is computed. In contrast to the existing methods the proposed method enables continuous damage parameter computation without the need of waiting for the cycles to close. The limitations of the standardized damage parameters are thus surpassed. The damage parameters derived initially for closed and isothermal cycles assuming that the elastoplastic stress–strain response follows the Masing and memory rules can now be used to take the mean stress effect into account under an arbitrary low cycle thermo-mechanical loading. The method includes:
This paper was originally published in the Methods X 1 (2014) 81–89.
Video presentations introducing modern thermal analysis.
Wearable textiles capture energy from body movement to generate electricity
Researchers have developed a bioplastic made from spirulina cells that is both stronger than previous versions and can degrade in a backyard compost bin.
Addition of titanium carbide-based materials significantly reduces friction and wear
Korean researchers investigate degradation of commercial materials in soil and seawater