DNA nanobiostructures
Volume 4, Issue 6, Page 30–39
| Rashid Bashir
Recent advances in the field of nanotechnology and nanobiotechnology have been fuelled by the advancement in fabrication technologies that allow construction of artificial structures that are the same size or smaller than many biological entities.