News
 

Scientists have developed a practical method for measuring the conductivity of a single carbon nanotube, by splitting it into two halves.

News
 

A novel platinum-gold alloy, 100 times more durable than high-strength steel, is believed to be the most wear-resistant metal in the world.

News
 

A novel graphene-assembled film possesses higher thermal conductivity than graphite film, even though graphite consists of many layers of graphene.