Interview with: Assistant Professor Jiaxing Huang, Northwestern University, USA
Researchers have shown that the atomic-level vibrations of graphene sheets coated in antibodies can be used to detect the SARS-CoV-2 virus.
Using 3D aerosol jet-printing, scientists have produced a highly sensitive X-ray detector by printing arrays of perovskite pillars on a graphene substrate.