A curved graphene ribbon, illustrated in grey, is shown laid flat against another graphene sheet. There is a continuous change in the twist angle between the ribbon above and the sheet below. In some places the atomic lattices of the two sheets line up at a 0° angle to each other, while in others, they are twisted relative to each other by as much as 5°. Image: Cory Dean, Columbia University.Think you know everything about a material? Try giving it a twist – literally. That’s the main idea behind an emerging field in condensed matter physics called ‘twistronics’, which has researchers drastically changing the properties of 2D materials like graphene by subtly changing the angles between stacked layers —as small as going from a 1.1° to 1.2°.
Twisted layers of graphene, for example, have been shown to behave in ways that single sheets do not. This includes acting like magnets, like electrical superconductors or like a superconductor’s opposite, insulators, all due to small changes in the twist angle between the sheets.
In theory, you could dial in any property by turning a knob that changes the twist angle. The reality, however, isn’t so straightforward, says Cory Dean, a physicist at Columbia University. Two twisted layers of graphene can become like a new material, but exactly why these different properties manifest is not well understood, let alone something that can be fully controlled.
Dean and his lab have now come up with a simple new fabrication technique that may help physicists probe the fundamental properties of twisted layers of graphene and other 2D materials in a more systematic and reproducible way. In a paper in Science, they report using long ‘ribbons’ of graphene, rather than square flakes, to create devices that offer a new level of predictability and control over both twist angle and strain.
Graphene devices have typically been assembled from atom-thin flakes of graphene that are just a few square millimeters in size. The resulting twist angle between the sheets is fixed in place, and the flakes can be tricky to layer together smoothly.
“Imagine graphene as pieces of saran wrap – when you put two pieces together you get random little wrinkles and bubbles,” says postdoc Bjarke Jessen, a co-author of the paper. Those bubbles and wrinkles are akin to changes in the twist angle between the sheets, and the physical strain that develops in between can cause the material to buckle, bend and pinch randomly. All these variations can yield new behaviors, but they have been difficult to control within and between devices.
Ribbons can help smooth things out. The lab’s new research shows that, with just a little push from the tip of an atomic force microscope, they can bend a graphene ribbon into a stable arc that can then be placed flat on top of a second, uncurved, graphene layer. The result is a continuous variation in the twist angle between the two sheets that spans from 0° to 5° across the length of the device, with evenly distributed strain throughout – no more random bubbles or wrinkles to contend with.
“We no longer have to make 10 separate devices with 10 different angles to see what happens,” said postdoc and co-author Maëlle Kapfer. “And we can now control for strain, which was completely lacking in prior twisted devices.”
The team used special high-resolution microscopes to confirm how uniform their devices were. With that spatial information, they developed a mechanical model that predicts twist angles and strain values based simply on the shape of the curved ribbon.
This first paper was focused on characterizing the behavior and properties of ribbons of graphene as well as other materials that can be thinned to single layers and stacked on top of each other. “It’s worked with every 2D material that we’ve tried so far,” noted Dean.
From here, the lab plans to use their new technique to explore how the fundamental properties of quantum materials change as a function of twist angle and strain. For example, prior research has shown that two twisted layers of graphene act like a superconductor when the twist angle is 1.1°. However, there are competing models to explain the origins of superconductivity at this so-called ‘magic angle’, as well as predictions of additional magic angles that have thus far been too difficult to stabilize, Dean said. With devices made with ribbons, which contain all angles between 0° and 5°, the team can more precisely explore the origins of this phenomenon, and others.
“What we are doing is like quantum alchemy: taking a material and turning it into something else,” said Jessen. “We now have a platform to systematically explore how that happens.”
This story is adapted from material from Columbia University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.