Current research
Volume 61, Pages 11–21Q. Chao, X.Y. Cui, Z.B. Chen, A.J. Breen, M. Cabral, N. Haghdadi, Q.W. Huang, R.M. Niu, H.S. Chen, B. Lim, S. Primig, M. Brandt, W. Xu, S.P. Ringer, X.Z. Liao
News
Improved high-voltage, hermetically sealed microbattery design
20 January 2023Laurie Donaldson
Current research
Volume 61, Pages 22–29Jianxin Cao, Xiaoye Luo, Shilian Yang, Fei Liu, Peng Chen, Shuang-Feng Yin
News
Researchers have developed an electrochemical transistor based on a new kind of electronic polymer and a vertical, instead of planar, architecture.
27 January 2023
Current research
Volume 61, Pages 30–39Seonmin Lee, Hyeokjoo Choi, Jihoon Bae, Seon-Hak Lee, Yoohan Ma, Seungsun Yoo, Jae-Hyun Ha, Jung-Il Hong, Seoyeon Park, Kyoohee Woo, Ji-Hyuk Choi, Sungwon Lee