Researchers have derived governing equations that describe and explain why adding liquid inclusions to elastomers gives them novel properties.
Researchers have created a simple-to-make, recyclable polymer fiber that can perform like a muscle actuator.
Unique properties of 2D materials stressed by contoured substrates
Researchers have found that adding the organometallic ferrocene to perovskite-based solar cells can dramatically increase their efficiency and stability.
Partnering with the Chinese Failure Analysis Institution (CFAI) of the Chinese Mechanical Engineering Society (CMES)