University of Wisconsin-Madison materials engineers have made a significant leap toward creating higher-performance electronics with improved battery life — and the ability to flex and stretch.
Led by materials science Associate Professor Michael Arnold and Professor Padma Gopalan, the team has reported the highest-performing carbon nanotube transistors ever demonstrated. In addition to paving the way for improved consumer electronics, this technology could also have specific uses in industrial and military applications.
Carbon nanotubes are single atomic sheets of carbon rolled up into a tube. As some of the best electrical conductors ever discovered, carbon nanotubes have long been recognized as a promising material for next-generation transistors, which are semiconductor devices that can act like an on-off switch for current or amplify current. This forms the foundation of an electronic device.
“The advance enables new types of electronics that aren’t possible with the more brittle materials manufacturers are currently using."Michael Arnold, materials science Associate Professor.
However, researchers have struggled to isolate purely semiconducting carbon nanotubes, which are crucial, because metallic nanotube impurities act like copper wires and “short” the device. Researchers have also struggled to control the placement and alignment of nanotubes. Until now, these two challenges have limited the development of high-performance carbon nanotube transistors.
Building on more than two decades of carbon nanotube research in the field, the UW-Madison team drew on cutting-edge technologies that use polymers to selectively sort out the semiconducting nanotubes, achieving a solution of ultra-high-purity semiconducting carbon nanotubes.
Previous techniques to align the nanotubes resulted in less-than-desirable packing density, or how close the nanotubes are to one another when they are assembled in a film. However, the UW-Madison researchers pioneered a new technique, called floating evaporative self-assembly, or FESA, which they described earlier in 2014 in the ACS journal Langmuir. In that technique, researchers exploited a self-assembly phenomenon triggered by rapidly evaporating a carbon nanotube solution.
The team’s most recent advance also brings the field closer to realizing carbon nanotube transistors as a feasible replacement for silicon transistors in computer chips and in high-frequency communication devices, which are rapidly approaching their physical scaling and performance limits.
“This is not an incremental improvement in performance,” Arnold says. “With these results, we’ve really made a leap in carbon nanotube transistors. Our carbon nanotube transistors are an order of magnitude better in conductance than the best thin film transistor technologies currently being used commercially while still switching on and off like a transistor is supposed to function.”
This story is reprinted from material from University of Wisconsin-Madison, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.