A computational study by researchers led by Giulia Galli at the University of Chicago’s Pritzker School of Molecular Engineering has predicted the conditions necessary for creating specific spin defects in silicon carbide. These findings, reported in a paper in Nature Communications, represent an important step towards identifying parameters for fabricating spin defects useful for quantum technologies.
Electronic spin defects in semiconductors and insulators are rich platforms for quantum computing, sensing and communication applications. Defects are impurities and/or misplaced atoms in a solid and the electrons associated with these atomic defects carry a spin. This quantum mechanical property can be used to provide a controllable qubit, the basic unit of operation in quantum technologies.
Yet the synthesis of these spin defects, typically achieved experimentally by implantation and annealing processes, is not yet well understood and, importantly, cannot yet be fully optimized. In silicon carbide – an attractive host material for spin qubits due to its industrial availability – different experiments have so far yielded different recommendations and outcomes for creating the desired spin defects.
“There hasn’t yet been a clear strategy to engineer the formation of spin defects to the exact specifications we want, a capability that would be highly advantageous for advancing quantum technologies,” says Galli, a professor of molecular engineering and chemistry and corresponding author of the paper. “So, we embarked on a long computational journey to ask the following question: Can we understand how these defects form by carrying out comprehensive atomistic simulations?”
Galli’s team – including Cunzhi Zhang, a postdoctoral researcher in Galli’s group, and Francois Gygi, a professor of computer science at the University of California, Davis – combined multiple computational techniques and algorithms to predict the formation of specific spin defects known as ‘divacancies’ in silicon carbide.
“Divacancies are created by removing a silicon and a carbon atom sitting close together in a silicon carbide solid,” explains Zhang. “We know from previous experiments that these types of defects are promising platforms for sensing applications.”
Quantum sensing could allow the detection of magnetic and electric fields and also reveal how complex chemical reactions occur, beyond what’s possible with today’s technologies. “To unlock quantum sensing capabilities in the solid-state, we first need to be able to create the right spin defects or qubits at the right location.” Galli says.
To find a recipe for predicting the formation of particular spin defects, Galli and her team combined several techniques to help them look at the movements of atoms and charges when a defect forms as a function of temperature.
“Typically, when a spin defect is created, other defects also appear and those may negatively interfere with the targeted sensing capabilities of the spin defect,” says Gygi, the main developer of the first-principles molecular dynamics code Qbox used in the team’s quantum simulations. “Being able to fully understand the complex mechanism of defect formation is very important.”
The team coupled the Qbox code with other advanced sampling techniques developed within the Midwest Integrated Center for Computational Materials (MICCoM), a computational materials science center headquartered at Argonne National Laboratory and funded by the US Department of Energy. Galli and Gygi are both senior investigators at MICCoM.
“Our combined techniques and multiple simulations revealed to us the specific conditions under which divacancy spin defects can be efficiently and controllably formed in silicon carbide,” Galli says. “In our calculations, we are letting the fundamental physics equations tell us what is happening inside the crystal structure when defects form.”
The researchers expect that experimentalists will be interested in using their computational tools to engineer a variety of spin defects in silicon carbide and other semiconductors. However, they caution that generalizing their tool to predict a broader range of defect formation processes and defect arrays will require more work. “But the proof of principle we have provided is important – we showed that we can computationally determine some of the conditions required to create the desired spin defects” Galli says.
Next, her team will continue working to expand their computational studies and speed up their algorithms. They also would like to expand their investigation to include a range of more realistic conditions. “Here, we’re only looking at samples in their bulk form, but in experimental samples there are surfaces, strain and also macroscopic defects,” Galli says. “We would like to include their presence in our future simulations and in particular understand how surfaces influence spin defect formation.”
Although her team’s advance is based on computational studies, Galli says all their predictions are rooted in long-standing collaborations with experimentalists. “Without the ecosystem we work in, constantly talking with and partnering with experimentalists, this wouldn’t have happened.”
This story is adapted from material from the University of Chicago, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.