New technology often calls for new materials – and with supercomputers and simulations, researchers no longer have to wade through inefficient guesswork to invent them from scratch.
The Materials Project, an open-access database founded at the US Department of Energy’s Lawrence Berkeley National Laboratory (Berkeley Lab) in 2011, computes the properties of both known and predicted materials. Researchers can focus on promising materials for future technologies –lighter alloys that improve fuel economy in cars, more efficient solar cells to boost renewable energy and faster transistors for the next generation of computers.
Now, Google DeepMind – Google’s artificial intelligence (AI) lab – is contributing nearly 400,000 new compounds to the Materials Project, expanding the amount of information researchers can draw upon. The dataset includes how the atoms of a material are arranged (the crystal structure) and how stable it is (formation energy).
“We have to create new materials if we are going to address the global environmental and climate challenges,” said Kristin Persson, the founder and director of the Materials Project at Berkeley Lab and a professor at the University of California (UC) Berkeley. “With innovation in materials, we can potentially develop recyclable plastics, harness waste energy, make better batteries and build cheaper solar panels that last longer, among many other things.”
To generate the new data, Google DeepMind developed a deep learning tool called Graph Networks for Materials Exploration (GNoME). Researchers trained GNoME using workflows and data that were developed over a decade by the Materials Project and improved the GNoME algorithm through active learning. GNoME researchers ultimately produced 2.2 million crystal structures, including 380,000 that they are adding to the Materials Project and predict are stable, making them potentially useful in future technologies. The new results from Google DeepMind are reported in a paper in Nature.
Some of the computations from GNoME were used alongside data from the Materials Project to test A-Lab, a facility at Berkeley Lab where AI guides robots in making new materials. A-Lab’s first paper, also published in Nature, showed that the autonomous lab can quickly discover novel materials with minimal human input.
Over 17 days of independent operation, A-Lab successfully produced 41 new compounds out of an attempted 58 – a rate of more than two new materials per day. For comparison, it can take a human researcher months of guesswork and experimentation to create one new material – if they ever reach the desired material at all.
To make the novel compounds predicted by the Materials Project, A-Lab’s AI created new recipes by combing through scientific papers and using active learning to make adjustments. Data from the Materials Project and GNoME were used to evaluate the materials’ predicted stability.
“We had this staggering 71% success rate, and we already have a few ways to improve it,” said Gerd Ceder, the principal investigator for A-Lab and a scientist at Berkeley Lab and UC Berkeley. “We’ve shown that combining the theory and data side with automation has incredible results. We can make and test materials faster than ever before, and adding more data points to the Materials Project means we can make even smarter choices.”
The Materials Project is the most widely used open-access repository of information on inorganic materials in the world. The database holds millions of properties on hundreds of thousands of structures and molecules, information primarily processed at Berkeley Lab’s National Energy Research Science Computing Center. More than 400,000 people are registered as users of the site and, on average, more than four papers citing the Materials Project are published every day. The contribution from Google DeepMind is the biggest addition of structure-stability data from a group since the Materials Project began.
“We hope that the GNoME project will drive forward research into inorganic crystals,” said Ekin Dogus Cubuk, lead of Google DeepMind’s Materials Discovery team. “External researchers have already verified more than 736 of GNoME’s new materials through concurrent, independent physical experiments, demonstrating that our model’s discoveries can be realized in laboratories.”
The Materials Project is now processing the compounds from Google DeepMind and adding them into the online database. The new data will be freely available to researchers, and also feed into projects such as A-Lab that partner with the Materials Project.
“I’m really excited that people are using the work we’ve done to produce an unprecedented amount of materials information,” said Persson, who is also the director of Berkeley Lab’s Molecular Foundry. “This is what I set out to do with the Materials Project – to not only make the data that I produced free and available to accelerate materials design for the world, but also to teach the world what computations can do for you. They can scan large spaces for new compounds and properties more efficiently and rapidly than experiments alone can.”
By following promising leads from data in the Materials Project over the past decade, researchers have experimentally confirmed useful properties in new materials across several areas. Some show potential for use as: carbon-capture materials (for pulling carbon dioxide from the atmosphere); photocatalysts (materials that speed up chemical reactions in response to light and could be used to break down pollutants or generate hydrogen); thermoelectrics (materials that could help harness waste heat and turn it into electrical power); and transparent conductors (which might be useful in solar cells, touch screens or LEDs).
Of course, finding these prospective materials is only one of many steps to solving some of humanity’s big technology challenges.
“Making a material is not for the faint of heart,” Persson said. “It takes a long time to take a material from computation to commercialization. It has to have the right properties, work within devices, be able to scale, and have the right cost efficiency and performance. The goal with the Materials Project and facilities like A-Lab is to harness data, enable data-driven exploration, and ultimately give companies more viable shots on goal.”
This story is adapted from material from Lawrence Berkeley National Laboratory, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.